Červenka Consulting

Prackovice Viaduct – Crack Analysis of a Segmental Bridge

Nonlinear analysis of diagonal web cracks in a prestressed segmental motorway viaduct and verification of the proposed strengthening.

Period: 2020 – 2022
Structure: motorway viaduct, prestressed concrete segmental box girder
Software: ATENA

The Prackovice viaduct on the D8 motorway (Lovosice – Řehlovice section) is a continuous prestressed concrete box girder 2.7 m deep with typical spans of 48 m. It was erected by the balanced cantilever method from segments with epoxy-glued joints. During and after construction, diagonal cracks 0.1 to 0.5 mm wide appeared in the webs of the second to fourth segment from the piers. The task was to find the probable cause of the cracking and to assess its effect on the load-carrying capacity.

The ATENA model covered a typical cantilever, i.e. one pier and half of each adjacent span, with the actual reinforcement, the bonded prestressing tendons and interface elements in the segment joints. The simulation followed the real construction schedule, creep and shrinkage, a one-day thermal event recorded during a construction break before the pavement was laid, and finally traffic load increased up to failure. All variants were calculated with mean and with characteristic material parameters.

The analysis showed that the cracks were caused mainly by the thermal event acting on the uncovered deck, together with the dead load and long-term effects, and strengthening of the segments next to the piers was recommended. In 2022 a follow-up analysis verified the strengthening design with external prestressed cables anchored in new deviators. The ultimate limit state was satisfied, and the computed maximum crack width in the web dropped from about 0.75 mm to about 0.40 mm, with no further crack growth expected during the service life.

Prackovice viaduct, view from below
The Prackovice viaduct.
ATENA finite element model of the bridge cantilever
ATENA model of a typical cantilever: longitudinal section with tendons and 3D view.
Crack width in the girder web before and after strengthening
Crack width in the girder web before and after strengthening, compared with a crack observed on the bridge.
Zeptejte se AI na program ATENA